All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
NC-4 Feldspar 12.00
Cedar Heights Goldart 26.00
Hawthorn Fireclay 20.00
Helmer Kaolin 12.00
XX Sagger 16.00
Silica 14.00

Instructions

Published in the July/August 2016 issue of Pottery Making Illustrated.