All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Laguna WC-617, #16 (in lbs) 1.00
Mason Stain (in tsp) 3.00

Instructions


*Use 3–5 tsp Mason stain per pound of clay.

Wearing gloves, form the ball of clay into a small pinch pot. Add the powdered stain inside the pot. Then knead or wedge until mixture is completely homogenized. Vary the amount of the Mason stain used based on the desired saturation.

 

This recipe was shared by Adrienne Eliades in the September/October 2021 issue of Pottery Making Illustrated.