All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Nepheline Syenite 22.49
Custer Feldspar 23.81
EPK 13.49
Zinc Oxide 22.77
Whiting 17.43
Add Amount
Red Iron Oxide 10.00

Instructions

This is a glaze from Tom Coleman from the book, "Glazes I Use".

Nice surface with interesting crystal growth.

 
The test tile is Coleman Porcelain fired in reduction.