All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Dolomite 4.70
Lithium Carbonate 2.00
Talc 8.00
Whiting 15.90
G-200 Feldspar 20.20
EPK 18.90
Flint 30.30
Tin Oixde 3.50

Instructions

Found in Ceramic Tech., Fall 2010.  Test tile is on B-Mix, fired in reduction.
Can be runny if applied thickly.