All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 20.00
Custer Feldspar 40.00
EPK Kaolin 10.00
Silica 30.00
Add Amount
Tin Oxide 1.50
Bentonite 3.00

Instructions

Published in "Cone 10 Glazes" by David MacDonald in the June/July/August 2017 issue of Ceramics Monthly.