All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Lithium Carbonate 95.00
Bentonite 5.00

Instructions


Paint this wash lightly over the glaze to encourage running. (Painted over EM Satin on selected areas of color and lines.) Recipe shared by Chandra DeBuse.

Commercial products used:

Amaco HF9 Zinc-Free Clear (painted over selected areas to keep glossy and crisp line)

Amaco Satin Matte Glazes: SM63 Yellow, SM27 Teal, SM42 Mint

Amaco Underglazes: V361 Jet Black for inlay, V375 Maroon

Duncan Premium Gold Luster

This recipe was shared by Stephanie Wilhelm in the November 2019 issue of Ceramics Monthly.