All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Ferro Frit 3110 57.69
Ferro Frit 3134 25.00
EPK Kaolin 7.19
Silica (325 Mesh) 10.12
Add Amount
Bentonite 2.02
Copper Carbonate 1.01

Instructions


Best when applied in a medium-thick application, equivalent to 3 pieces of construction paper stacked on top of one another.

This recipe was shared by Lisa Orr in the November 2019 issue of Ceramics Monthly.