All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Ferro Frit 3124 22.00
6 Tile Kaolin 62.50
Newman Red Clay 15.50

Instructions


This recipe was shared by Katie Fee in the March 2021 issue of Ceramics Monthly.