Limestone Glaze Moloney Hi

You have read of of your complimentary recipes for the month.
For unlimited access to Ceramics Recipes premium content, please subscribe.
Yes, I want to subscribe to Ceramics RecipesAlready a digital subscriber? Log in now.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.

Please enjoy this complimentary recipe for the month.
For unlimited access to Ceramics Recipes premium content, please subscribe.
Yes, I want to subscribe to Ceramics RecipesNot right now. Continue to recipe. Already a digital subscriber? Log in now.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.

Subscribe
Ingredients
Instructions
Published in "Mary Cay's Glittering Obsession" by Sumi von Dassow, in the Feb 2006 issue of Ceramics Monthly.
Stains can be added to this glaze according to the manufacturer’s recommendations. For Yellow Glaze Kiln Jewels, 3% Cerdec yellow stain was added.
Carbonates and oxides also have been added to this recipe with success by using various proportions. A strong cobalt glaze was mixed with this glaze to produce the Sky Blue Glaze Kiln Jewel, but cobalt carbonate or oxide also could be used.
A wash of copper sulfate can be sprayed or brushed on to create the Copper Sulfate Glaze Kiln Jewels.
Recipe Topics
Clay Bodies and Casting Slips
Low Fire (Cone 022 – 01)
Mid Range (Cone 1 – 7)
High Fire (Cone 8 – 14)
Raku
Salt, Soda, and Wood
Slip, Engobe, and Terra Sigillata
Reference
Create your own Recipes!
You can keep your recipes private or share with others.
Create a Recipe
Manage your Recipes