All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 20.00
Custer Feldspar 40.00
EPK Kaolin 10.00
Silica 30.00
Add Amount
Zircopax 10.00
Cobalt Carbonate 0.50
Red Iron Oxide 1.00

Instructions


I use this glaze on the rim of cups layered under San Miguel Icy Blue to create a watery, dripping effect.

This recipe was shared by Mark Chuck in the June/July/August 2019 issue of Ceramics Monthly.