All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Washed Hardwood Ash 40.00
Custer Feldspar 40.00
OM 4 Ball Clay 20.00
Add Amount
Bentonite 2.00

Instructions

Published in the July/August 2016 issue of Pottery Making Illustrated.

The image here shows a piece with Matthew Krousey's Bisque Slip (applied on bisque ware before glazing), Iron Wash (the dark lines), and Leach Ash Glaze.