All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Magnesium Carbonate 25.00
Talc 15.00
Ferro Frit 3195 10.00
Soda Feldspar 35.00
Kaolin 15.00
Add Amount
Cobalt Carbonate 2.50

Instructions


This recipe was sourced from The Ceramic Spectrum: A Simplified Approach to Glaze and Color Development by Robin Hopper. Shared in the December 2020 issue of Ceramics Monthly.