All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Custer Feldspar 16.72
HB Fire Clay (20 and 35 mesh) 41.64
6 Tile Kaolin 41.64
Add Amount
Sand 16.60
*Cedar Heights Redart Clay 10.00

Instructions

Published in "Clay & Glaze: Low to High" by Bede Clarke, in the Sep 2014 issue of Ceramics Monthly.
*Add 10-20%  Cedar Heights Redart Clay to the clay body for added color.