All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Cedar Heights Redart 1200.00
Distilled Water 2800.00
Add Amount
Sodium Silicate 6.50

Instructions

This recipe was shared by Ben Jordan in the May 2018 issue of Ceramics Monthly.
Clay and water measurements are in grams.

This terra sigillata fluxes a lot and loses some burnished quality, but can still work at cone 6.