All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Ferro Frit 3195 40.00
EPK Kaolin 60.00
Add Amount
Bentonite 10.00

Instructions


This recipe was shared by Justin Rothshank in his book Low-Fire Soda, available in the Ceramic Arts Network shop: https://mycan.ceramicartsnetwork.org/s/product-details?id=a1B3u000009udqwEAA.