All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Kentucky Stone 43.40
Tile 6 Kaolin 17.10
Hawthorne Fire Clay 26.30
Foundry Sand (80 mesh) 13.20

Instructions

Published in "Search for True Shino" by Stephen Driver with Judith and Royle Duff in the December 2016 issue of Ceramics Monthly.

Judith Duff's clay body. Shown in the image here with Judith Duff Shino Glaze #1.
Duff developed this glaze to replicate the qualities she appreciated in Japanese Mogusa clay.