All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Nepheline Syenite 30.00
EPK Kaolin 10.00
Grolleg Kaolin 50.00
Newman Red Clay 10.00
Add Amount
Bentonite 3.00

Instructions

Developed by Randy Johnston, this classic yellow to orange to red flashing slip works well in both wood and soda atmospheres.