All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Custer Feldspar 43.00
Whiting 21.00
EPK Kaolin 10.00
Silica 26.00
Add Amount
Red Iron Oxide 16.00
Bentonite* 3.00

Instructions

Published in "Firing Up and Down" by Deklan Ranlett, in the Jan/Feb 2014 issue of Pottery Making Illustrated.
*Weigh the Bentonite separately and dry mix it with the other ingredients before adding water.