All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Talc 10.00
Whiting 10.00
Ferro Frit 3134 10.00
Ferro Frit 3195 10.00
Custer Feldspar 10.00
Spodumene 10.00
Ball Clay 10.00
Kaolin 10.00
Silica (200 mesh) 10.00
Silica (325 mesh) 10.00

Instructions

This recipe was used to test the opacifiers Zircopax, Tin Oxide, and Titanium Dioxide, from 2–10%. The image shown here displays the range of results.

Published in "Opacifiers" by Dave Finkelnburg, in the Oct 2014 issue of Ceramics Monthly.