All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Dolomite 25.80
Whiting 4.50
Custer Feldspar 32.60
Soda Feldspar 22.50
Kaolin 14.60
Add Amount
Titanium Dioxide 10.00
Nickel Oxide 2.20

Instructions

Published in "Cone 10 Glazes" by Holly Hanessian, in the Feb 2017 issue of Ceramics Monthly.
This glaze works best when applied to about the thickness of a credit card. The nickel oxide in the glaze can fume and affect glazes on surrounding pieces during the firing.