All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 34.00
Custer Feldspar 46.00
EPK Kaolin 20.00
Add Amount
Copper Carbonate 5.00

Instructions

This recipe was published in the June/July/August 2018 issue of Ceramics Monthly.
Mix the glaze to a half-and-half consistency.