All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Custer Potash Feldspar 60.00
Dolomite 20.00
Flint 18.00
Grolleg 3.00
Add Amount
Rutile 3.00
Cobalt Oxide 2.00

Instructions


stir well