All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Bone Ash 1.87
Dolomite 26.66
Talc 1.87
Whiting 12.16
Minspar 200 Feldspar 32.65
Georgia Kaolin 24.79
Add Amount
Zircopax 5.61
Red Iron Oxide 2.64

Instructions


Mix the glaze to a half-and-half consistency. I use slip under JVM Orange to achieve a yellow color.