All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Kona F-4 Feldspar (sub. Minspar 200 Fledspar) 25.00
OM 4 Ball Clay 31.00
6 Tile Kaolin 31.00
Silica 12.00
Add Amount
Red Iron Oxide 8.00
Bentonite 4.00

Instructions


This slip is mixed to buttermilk consistency for this application.

This recipe was shared by Jeff Diehl in the May 2020 issue of Ceramics Monthly.