All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gillespie Borate 50.00
Red Iron Oxide 50.00

Instructions

This recipe was contributed by Elena Renker in the November 2019 issue of Ceramics Monthly.
I add Sussett (Peptapon #52) to this slip for better brushability. Sussett is an organic gum powder (like CMC Gum) that is mixed with boiling water in a ratio of 20g powder to 1 quart (1L) water. It forms a gel that can be mixed with glazes. Add 4 tsp. (20 mL) of Sussett gel per 1 quart (1L) of glaze.