All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Ofuyu Stone 60.00
Azuma Ash Clay 32.00
Silica 8.00

Instructions

Published in "Satori Yamaoka" by Bob McWilliams, in the May 2005 issue of Ceramics Monthly.