All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Ferro Frit 3134 50.00
EPK Kaolin 30.00
Silica 20.00
Add Amount
Mason Stain 6088 Dark Red 5.00
Mason Stain 6666 Black 8.00

Instructions


This is a runny clear glaze. I brush it on thickly to get bigger drips.

This recipe was shared by Jill Birschbach in the September 2020 issue of Ceramics Monthly.