All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 14.46
Minspar 200 Feldspar 71.08
Silica 14.46
Add Amount
Zinc Oxide 9.64
Red Iron Oxide 9.64
Rutile 1.93

Instructions


This recipe works well in wood, soda, and gas-reduction firings. It can be used as a glaze and a thin wash.

This recipe was shared by Justin Rothshank in the March 2019 issue of Ceramics Monthly.