All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 31.25
Albany Slip 50.00
Ball Clay 18.75
Add Amount
Cobalt Carbonate 1.56
Iron Oxide 1.56

Instructions

Albany Slip is no longer available, but try substituting another high-iron slip clay like Barnard.

Published in "Lenore Vanderkooi" by Phyllis Blair Clark, in PMI a CM Supplement 1998.