All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Strontium Carbonate 10.00
Whiting 30.00
Cedar Heights Redart 60.00
Add Amount
Red Iron Oxide 3.50
Yellow Ochre 4.00

Instructions

The rivulets in this glaze come from high surface tension in the melted glaze while also being very runny.

Published in "The Studio Sale" by David Cuzick, in the Sept 2000 issue of Ceramics Monthly.
Spray onto porcelain.  Very fluid at Cone 10, so be careful to not overfire.