All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Ferro Frit 3124 30.00
EPK Kaolin 30.00
Gerstley Borate 40.00

Instructions

Published in "3 Ingredient Glazes" by Holly Goring, in the Sep/Oct 2011 issue of Pottery Making Illustrated.