All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 5.00
Lithium Carbonate 80.00
EPK Kaolin 10.00
Silica 5.00
Add Amount
Zircopax 6.00
Mason Stain 6374 Turquoise 5.00

Instructions

This recipe was originally published in the January/February 2018 issue of Pottery Making Illustrated.
This glaze is crystallized with a lot of sparkle. The crust floats and moves on the pieces during the firing. This glaze is creepy and beautiful at the same time. Definitely worth investigation if you’re making sculptural work. Not food safe.