All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Minspar 200 Feldspar 28.00
Grolleg Kaolin 53.00
Silica 19.00
Add Amount
Macaloid 3.00

Instructions

Published in "Emerging Artist Recipes" in the May 2017 issue of Ceramics Monthly.