All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 55.00
EPK Kaolin 30.00
Silica 15.00
Add Amount
Rutile 3.00

Instructions

Originally published in the Nov/Dec issue of Pottery Making Illustrated.