All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Cornwall Stone 42.00
Dolomite 15.00
Whiting 10.00
EPK Kaolin 23.00
Silica 10.00
Add Amount
Yellow Ochre 6.00
Cobalt Carbonate 2.00
Chrome Oxide 1.00

Instructions

Published in "Soft Slab Teapot" by Margaret Bohls, in the Mar/Apr 2010 issue of Pottery Making Illustrated.