All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 32.67
Wollastonite 2.97
Strontium Carbonate 2.97
Ferro Frit 3110 30.70
EPK Kaolin 25.74
Silica (325 mesh) 4.95
Add Amount
Bentonite 2.00
Red Iron Oxide 6.00

Instructions

This glaze is food safe and translucent. Test in Your own kiln with your materials and firing schedule to determine food safety, as results may be different.

Published in "Low-Fire Surfaces" by Ronan Kyle Peterson, in the September 2017 issue of Ceramics Monthly.