Exterior Glaze - Robbie's Y Glaze David Pier

You have read of of your complimentary recipes for the month.
For unlimited access to Ceramics Recipes premium content, please subscribe.
Yes, I want to subscribe to Ceramics RecipesAlready a digital subscriber? Log in now.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.

Please enjoy this complimentary recipe for the month.
For unlimited access to Ceramics Recipes premium content, please subscribe.
Yes, I want to subscribe to Ceramics RecipesNot right now. Continue to recipe. Already a digital subscriber? Log in now.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.

Subscribe
Ingredients
Instructions
This has been altered from Karen's Y Glaze, which uses G-200 feldspar instead of Custer Feldspar and rutile instead of titanium dioxide. All percentage weight amounts are the same.
Published in "Flameware" by David Pier, in the May 2011 issue of Ceramics Monthly.
Note: No guarantee is made by the author or CeramicRecipes.org regarding these recipes. All individuals must test materials and maintain quality control to ensure proper performance of any clay body - particularly flameware. To test if you actually have flameware after you fire it, don full protective clothing including a mask with a face shield and apply a propane torch flame directly to one spot on the test piece. Once it gets red hot, pick it up with tongs and drop it in a metal bucket of water. If it can take that, then it is flameware. You still need to be careful because you can never be sure there aren't any pores that may create steam pressure in the future.
Recipe Topics
Clay Bodies and Casting Slips
Low Fire (Cone 022 – 01)
Mid Range (Cone 1 – 7)
High Fire (Cone 8 – 14)