All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 21.00
Whiting 20.00
Nepheline Syenite 16.00
EPK Kaolin 11.00
Silica 32.00
Add Amount
Chromium Oxide 0.20

Instructions

Published in "Gemstones & Glazes" by Ryan Coppage, in the Sep 2017 issue of Ceramics Monthly.

This is a fluid glaze that runs if thick, but does not craze.