All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
OM 4 Ball Clay 25.00
EPK Kaolin 25.00
Nepheline Syenite 25.00
Silica 25.00
Add Amount
Cobalt Carbonate or Oxide 0.53

Instructions

Shown here with Red Brown Trailing Slip and Lau Luster Shino over top.

Published in "Ed Thompson's Slip Marbling" by Richard Burkett, in the Jan/Feb 2003 issue of Pottery Making Illustrated.