All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Talc 10.00
Nepheline Syenite 5.00
Carbondale Red Clay 10.00
Hawthorn Bond Fire Clay 25.00
Cedar Heights Redart Clay 50.00
Add Amount
*Sand 5.00

Instructions

Published in "Clay & Glaze: Low to High" by Bede Clarke, in the Sep 2014 issue of Ceramics Monthly.
*Add 5-10% sand to the clay body.