All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Borax 36.00
Ferro Frit 3195 8.00
Cullet (from clear bottles) 56.00
Add Amount
Cobalt Carbonate 2.00

Instructions

Published in "Letters" in the Sept 2012 issue of Ceramics Monthly.
The addition of small percentages of iron oxide, rutile, or manganese dioxide will yield a varied palette of greens and browns.