All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Custer Feldspar 5.88
A.P. Green Fireclay 23.53
Cedar Heights Goldart 23.53
Cedar Heights Redart 23.53
Kentucky Ball Clay (OM 4) 17.65
Mullite (48 mesh) 5.88

Instructions

Published in "Rebecca Coffman" by Nancy McCrosky, in the May 2003 issue of Ceramics Monthly.