All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Ferro Frit 3134 29.13
Ferro Frit 3195 43.69
EPK Kaolin 24.27
Silica 2.91
Add Amount
CMC Gum 0.58
Veegum 1.55
Copper Carbonate 3.88

Instructions


Adding CMC Gum makes this glaze easy to brush.

This recipe was shared by Kari Radasch in the March 2019 issue of Ceramics Monthly.