Deboos Clear Susan McKinnon

You have read of of your complimentary recipes for the month.
For unlimited access to Ceramics Recipes premium content, please subscribe.
Yes, I want to subscribe to Ceramics RecipesAlready a digital subscriber? Log in now.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.

Please enjoy this complimentary recipe for the month.
For unlimited access to Ceramics Recipes premium content, please subscribe.
Yes, I want to subscribe to Ceramics RecipesNot right now. Continue to recipe. Already a digital subscriber? Log in now.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.

Subscribe
Ingredients
Instructions
Published in "Atmospheric Recipes," in the October 2018 issue of Ceramics Monthly. This recipe has been used by Susan McKinnon.Add a pinch of Epsom salts to the glaze to improve consistency. Tone will vary for each of the Mason stains (MS) with different atmospheres. In reduction, the green is brighter but in oxidation it is an olive shade. In oxidation, the blue is very pale, but in reduction the color is brighter.
Recipe Topics
Clay Bodies and Casting Slips
Low Fire (Cone 022 – 01)
Mid Range (Cone 1 – 7)
High Fire (Cone 8 – 14)
Raku
Salt, Soda, and Wood
Slip, Engobe, and Terra Sigillata
Reference
Create your own Recipes!
You can keep your recipes private or share with others.
Create a Recipe
Manage your Recipes