All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Bone Ash 1.00
Talc 3.00
Whiting 15.00
Zinc Oxide 2.00
Ferro Frit 3110 17.00
Nepheline Syenite 35.00
Silica 27.00
Add Amount
Tin Oxide 1.50
Titanium Dioxide 3.00
Copper Carbonate 1.50

Instructions

Originally published in the October 2010 issue of Ceramics Monthly.