All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Colemanite 5.09
Dolomite 13.40
Whiting 9.41
Custer Feldspar 25.45
Edgar Plastic Kaolin 19.50
Kentucky Ball Clay 1.70
Silica 25.45
Add Amount
Red Iron Oxide 0.85
Rutile 6.73

Instructions

Published in "The Studio Sale" by David Cuzick, in the Sep 2000 issue of Ceramics Monthly.