All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 10.00
Unwashed Wood Ash (mostly pine & ash) 40.00
Cullet 30.00
Ball Clay 15.00
Local Iron Rock (ground with mortar & pestle) 5.00

Instructions

Published in "In Historical Context" by Stephen Hawks, in the Nov 2001 issue of Ceramics Monthly.