All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Laguna Borate 80.00
Nepheline Syenite 20.00
Add Amount
Bentonite 3.00

Instructions

Published in "Precision Piercing" in the January/February 2016 issue of Pottery Making Illustrated.

A low-fire, raku glaze.
I use a gum solution in small amounts, as needed, and do not add it to the full batch of glaze.