All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 2.55
Talc 3.88
Whiting 18.06
Custer Feldspar 44.90
Cedar Heights Redart 11.33
OM 4 Ball Clay 6.22
Silica 13.06
Add Amount
Cobalt Oxide 1.00
Rutile 3.00

Instructions

Published in the March 2018 issue of Ceramics Monthly.

This recipe is from John Britt’s book, The Complete Guide to Mid-Range Glazes. The recipe was altered with progressive additions of cobalt oxide and rutile.