All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 80.00
Nepheline Syenite 20.00
Add Amount
Black Copper Oxide 3.00
Cobalt Oxide 1.00

Instructions

Published in "Geometric Glazing" by Sally Giarratana, in the Spring 1998 Pottery Making Illustrated.